Polymer Property : Izod Impact, Unnotched = 21.36 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® 500 PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance.
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® 500 PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance.
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® 500R PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release.
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® 500R PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release.
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® 503 PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized.
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized.
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® 503R PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release.
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® 503R PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release.
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC (Asia Pacific)
LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Easy Molding.
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DL003EU PC
LNP LUBRICOMP* DL003EU is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, UV Stabilized, Internally Lubricated.
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC
LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, Internally Lubricated