Izod Impact, Unnotched 12.97 J/cm
24.30 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOTUF PF00AIS PA 6 (Asia Pacific)
LNP* THERMOTUF* PF00AIS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Unnotched 12.97 J/cm
24.30 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOTUF PF00AIS PA 6
LNP THERMOTUF* PF00AIS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.