Polymer Property : Izod Impact, Unnotched = 24.4 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 24.4 J/cm
45.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics ULTEM AUT210 PEI
Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti..
Izod Impact, Unnotched 24.4 J/cm
45.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific)
Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o..
Izod Impact, Unnotched 24.4 J/cm
45.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics ULTEM AUT210 PEI (Europe-Africa-Middle East)
Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o..