Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 13.45 J/cm | 25.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 13.45 J/cm | 25.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific) LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 13.45 J/cm | 25.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF009H PA 66 LNP* THERMOCOMP* RF009H is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Izod Impact, Unnotched | 13.45 J/cm | 25.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF009H PA 66 (Asia Pacific) LNP* Thermocomp* RF009H is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched | 13.45 J/cm | 25.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |