Mechanical Properties Metric English Comments
Izod Impact, Unnotched 15.17 J/cm
28.42 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF009S PA 66 (Asia Pacific)
LNP* Thermocomp* RF009S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.