Polymer Property : Izod Impact, Unnotched = 3.15 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.15 J/cm
5.90 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Izod Impact, Unnotched 3.15 J/cm

@Temperature 23.0 °C
5.90 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC
LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup..
Izod Impact, Unnotched 3.15 J/cm
5.90 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC
LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant.
Izod Impact, Unnotched 3.15 J/cm
5.90 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific)
LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 3.15 J/cm
5.90 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS
LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Izod Impact, Unnotched 3.15 J/cm
5.90 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Izod Impact, Unnotched 3.15 J/cm

@Temperature 23.0 °C
5.90 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC (Asia Pacific)
LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup..
Izod Impact, Unnotched 3.15 J/cm

@Temperature -30.0 °C
5.90 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East)
VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin.