Polymer Property : Izod Impact, Unnotched = 3.75 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.60 - 2.00 J/cm

@Temperature 23.0 °C
3.00 - 3.75 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RH 225 Rigid PVC, Antishock Extrusion
Antishock pipes and profiles
Copyright © lookpolymers.com All Rights Reserved