Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.81 J/cm
7.14 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP KFP032 Acetal Copolymer
LNP LUBRICOMP* KFP032 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched 3.81 J/cm
7.14 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF003AXH PA 66
LNP* THERMOCOMP* RF003AXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material includes: Healthcare.
Izod Impact, Unnotched 3.81 J/cm
7.14 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP
LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.