Polymer Property : Izod Impact, Unnotched = 30.20 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 16.12 J/cm

@Temperature 23.0 °C
30.20 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubriloy D20001 PC
LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.This data was supplied by..
Izod Impact, Unnotched 16.12 J/cm
30.20 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific)
LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.