Polymer Property : Izod Impact, Unnotched = 33.31 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 17.78 J/cm
33.31 ft-lb/in
ASTM D4812
PlastiComp Complet® LGF60-PA66 MT 60% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.