Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.14 J/cm | 4.01 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 104 Polypropylene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 2.14 J/cm | 4.01 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 628 Nylon 6/6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |