Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.24 J/cm @Temperature 23.0 °C |
7.94 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp OFG26XXP PPS - Linear LNP* Lubricomp* OFG26XXP is a compound based on Linear PPS containing Glass Fiber and Graphite Powder. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for.. |