Mechanical Properties Metric English Comments
Izod Impact, Unnotched 21.89 J/cm
41.01 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 (Asia Pacific)
LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder, Impact Modifier. Added features of this material include: Electrically Conductive, High Impact.