Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 23.42 J/cm | 43.88 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 23.42 J/cm | 43.88 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC (Asia Pacific) LNP* Stat-kon* DX04490 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |