Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.534 - 2.94 J/cm
1.00 - 5.51 ft-lb/in
Average value: 1.67 J/cm Grade Count:19
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..