Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.73 J/cm | 10.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched | 5.73 J/cm | 10.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Asia Pacific) LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched | 5.73 J/cm | 10.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Europe-Africa-Middle East) LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched | 5.73 J/cm @Temperature 23.0 °C |
10.7 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp DFZ42P PC (Asia Pacific) LNP* Thermocomp* DFZ42P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the.. |