Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.09 J/cm @Thickness 3.18 mm |
11.4 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® LC-1006 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Unnotched | 6.09 J/cm | 11.4 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 114 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 6.09 J/cm | 11.4 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Aqualoy® 143 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |