Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.29 J/cm | 6.16 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP EX07305 PEI (Asia Pacific) Polyetherimide reinforced with Glass fiber and PTFE for use in Burn-in Test Sockets (BiTS) Application |
|||
Izod Impact, Unnotched | 3.29 J/cm | 6.16 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |