Polymer Property : Izod Impact, Unnotched = 6.65 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.55 J/cm
6.65 ft-lb/in
MD; ASTM D256
DuPont™ Nomex® Type 994, 250 mil Nominal Thickness Rigid Aromatic Nylon Board
Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T..