Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.64 J/cm | 6.82 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS LNP* THERMOCOMP* AF004L is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Low Extractible. |