Polymer Property : Izod Impact, Unnotched = 6.93 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.70 - 3.70 J/cm

@Temperature -40.0 - -40.0 °C
6.93 - 6.93 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 3.70 J/cm Grade Count:2
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..