Polymer Property : Izod Impact, Unnotched = 7.19 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.84 J/cm

@Thickness 3.18 mm
7.19 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Lubricomp® PDX-O-90351 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Izod Impact, Unnotched 3.84 J/cm
7.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP OX90351 PPS
LNP LUBRICOMP* OX90351 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched 3.84 J/cm
7.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON CD000I PS (Asia Pacific)
LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Izod Impact, Unnotched 3.84 J/cm
7.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET
LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications.
Izod Impact, Unnotched 3.84 J/cm

@Temperature 23.0 °C
7.19 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 3.84 J/cm

@Temperature 23.0 °C
7.19 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 (Asia Pacific)
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched 3.84 J/cm
7.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly
LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible.
Izod Impact, Unnotched 3.84 J/cm
7.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific)
LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible.
Izod Impact, Unnotched 3.84 J/cm
7.19 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 263 Glass Reinforced, Modified SMA
Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.