Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.37 J/cm | 13.8 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 464 Glass Fiber/Bead Reinforced, PET Alloy Data provided by the manufacturer, ComAlloy International Company.25% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 7.37 J/cm | 13.8 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 630 Nylon 6/6, Glass/Mineral Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |