Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.52 J/cm | 14.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.52 J/cm | 14.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DX10311 PC (Asia Pacific) DX10311 is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Izod Impact, Unnotched | 7.52 J/cm | 14.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF006L PA 66 LNP* THERMOCOMP* RF006L is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Izod Impact, Unnotched | 7.52 J/cm | 14.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF006L PA 66 (Asia Pacific) LNP* Thermocomp* RF006L is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Izod Impact, Unnotched | 7.52 J/cm | 14.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF006LXP PA 66 LNP* THERMOCOMP* RF006LXP is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Low Extractible. |