Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 4.06 J/cm
7.60 ft-lb/in
ASTM D4812
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved