Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.13 J/cm
7.74 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP ECL36XXQ PEI
LNP* Lubricomp* ECL36XXQ is a compound based on Polyetherimide containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 4.13 J/cm
7.74 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES
LNP THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing 20% Glass Fiber.
Izod Impact, Unnotched 4.13 J/cm
7.74 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Asia Pacific)
LNP* THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber.