Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.88 J/cm | 14.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF007H PA 66 LNP* Thermocomp* RF007H is a compound based on Nylon 66 containing glass fiber. Added feature includes: Healthcare. |
|||
Izod Impact, Unnotched | 7.88 J/cm | 14.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXP PA 66 LNP* THERMOCOMP* RF007SXP is a compound based on Nylon 66 containing 35% Glass Fiber. Added feature of this material includes: Heat Stabilized. |
|||
Izod Impact, Unnotched | 7.88 J/cm | 14.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UF00ASW PPA LNP* Thermocomp* UF00ASW is a compound based on Polyphthalamide (PPA) containing glass fiber. Characteristics of this grade of Heat Stabilized and Hot Water Moldable. |