Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.21 J/cm
7.89 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP KONDUIT ITF2B PA 6/12 (Asia Pacific)
LNP* Konduit* ITF2B is a compound based on Nylon 6/12 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Izod Impact, Unnotched 4.21 J/cm
7.89 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66
LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched 4.21 J/cm
7.89 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific)
LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 4.21 J/cm
7.89 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU
LNP THERMOCOMP* GF006 is a compound based on Polysulfone resin containing 30% Glass Fiber.
Izod Impact, Unnotched 4.21 J/cm
7.89 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP GF006XXZ PSU
LNP THERMOCOMP* GF006XXZ is a compound based on Polysulfone resin containing 30% Glass Fiber.
Izod Impact, Unnotched 4.21 J/cm

@Temperature 23.0 °C
7.89 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp RFZ42 PA 66
LNP* Thermocomp* RFZ42 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 4.21 J/cm
7.89 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP UCF22S PPA
LNP* Thermocomp* UCF22S is a compound based on Polyphthalamide resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive..
Izod Impact, Unnotched 4.21 J/cm

@Temperature 23.0 °C
7.89 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp RFZ42 PA 66 (Asia Pacific)
LNP* Thermocomp* RFZ42 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass.This data was supplied by SABIC-IP for the Asia Pacific region.