Polymer Property : Izod Impact, Unnotched = 7.92 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.23 J/cm
7.92 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 7062HP PBT
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Izod Impact, Unnotched 4.23 J/cm
7.92 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP (Asia Pacific)
LNP* Thermocomp* MF001AS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Unnotched 4.23 J/cm
7.92 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Izod Impact, Unnotched 4.23 J/cm
7.92 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Izod Impact, Unnotched 4.23 J/cm
7.92 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP
LNP* THERMOCOMP* MF001AS is a compound based on Polypropylene resin containing 5% Glass Fiber. Added features of this material include: Heat Stabilized.