Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.60 J/cm | 16.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin containing 10% Glass Fiber. |