Polymer Property : Izod Impact, Unnotched = 9.07 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.84 J/cm
9.07 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK
LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched 4.84 J/cm
9.07 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DE006ER PC
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
Izod Impact, Unnotched 4.84 J/cm
9.07 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific)
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.