Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.80 - 9.20 J/cm @Temperature 23.0 °C |
16.5 - 17.2 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 214 Rigid PVC, Antishock Extrusion Antishock rolling shutters |
|||
Izod Impact, Unnotched | 8.80 - 9.20 J/cm @Temperature 23.0 °C |
16.5 - 17.2 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 704 Rigid PVC, Antishock Extrusion Antishock spiral pipes |
|||
Izod Impact, Unnotched | 8.80 - 9.20 J/cm @Temperature 23.0 °C |
16.5 - 17.2 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds ARC 30 Rigid PVC, Atoxic for General Purpose Bottles very high antishock |