Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.32 J/cm @Thickness 3.17 mm |
17.4 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3027IR Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Izod Impact, Unnotched | 9.32 J/cm @Thickness 3.17 mm |
17.4 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3030I Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Izod Impact, Unnotched | 9.32 J/cm @Thickness 3.17 mm |
17.4 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3030IR Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Izod Impact, Unnotched | 9.32 J/cm @Thickness 3.17 mm |
17.4 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3030U Polycarbonate, UV Stabilized TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |