Tensile Strength at Break 0.0814 MPa
11.8 psi
Zeon Chemicals Nipol® P70 Polyblend Nitrile Elastomer
Nipol P70 is a 70/30 fully-fluxed polyblend of medium-high acrylonitrile content.A 70/30 fully fluxed nitrile-PVC blend. Provides outstanding ozone resistance. Used in cable jackets, hose, and shoe ..