Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 0.620 MPa | 89.9 psi | ASTM D3574 |
3M 4504 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Tensile Strength at Break | 0.620 MPa | 89.9 psi | Die "A"; ASTM D3759 |
3M 4504 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Tensile Strength at Break | 0.620 MPa | 89.9 psi | |
3M 4004 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |