Polymer Property : Tensile Strength at Break = 0.650 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.650 MPa
94.3 psi
ASTM D3574
3M 4718 Foam Tape
Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio..
Tensile Strength at Break 0.650 MPa
94.3 psi
Die "A"; ASTM D3759
3M 4718 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..