Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 0.862 MPa | 125 psi | ASTM D412 |
Parker Chomerics CHO-FORM 5528 Conductive Form-In-Place Gaskets Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |