Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.064 MPa | 154.3 psi | ASTM D4325 |
3M Scotch™ 23 Rubber Splicing Tape Scotch® Rubber Splicing Tape 23 is a highly conformable, self-fusing EPR (Ethylene Propylene Rubber) based, high voltage splicing tape. It is a non-vulcanizing, shelf-stable tape with excellent ele.. |