Polymer Property : Tensile Strength at Break = 1.11 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.11 MPa
161 psi
Change in tensile strength after 18 hours at 250°F, in animal fat; ASTM D471
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..