Tensile Strength at Break 1.30 MPa
189 psi
ISO 37
Premix Thermoplastics PRESEAL® TPE 5020
General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o..
Tensile Strength at Break 1.30 MPa
189 psi
ASTM D638
Premix Thermoplastics PRESEAL® TPE 5020
General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o..
Tensile Strength at Break 1.30 MPa
189 psi
Tensile stress at break.
Dow AFFINITY™ SM 8400 Polyolefin Elastomer
Data provided by Dow Chemical.