Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.61 MPa | 234 psi | 250 mm/min; ASTM D412A |
PolyOne Elastamax™ XL 0141-66 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |