Mechanical Properties Metric English Comments
Tensile Strength at Break 1.74 MPa
252 psi
50% RH
3M 4000 UV 5280 Marine Adhesive/Sealant Fast Cure
3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio..
Tensile Strength at Break 1.74 MPa
252 psi
50% RH
3M 4000 UV 6580 Marine Adhesive/Sealant Fast Cure
3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio..
Tensile Strength at Break 1.74 MPa
252 psi
50% RH
3M 4000 UV 6586 Marine Adhesive/Sealant Fast Cure
3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio..