Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.32 MPa @Treatment Temp. 121 °C, Time 64800 sec |
1497 psi @Treatment Temp. 250 °F, Time 18.0 hour |
in ASTM #2 Oil |
DuPont Elvax® 40L-03 Low Smoke Non-halogen Jacket Formulation
(discontinued **) Elvax® 40L-03 low smoke non-halogen jackets.Information provided by DuPont. |
|||
Tensile Strength at Break | 10.32 MPa @Treatment Temp. 121 °C, Time 64800 sec |
1497 psi @Treatment Temp. 250 °F, Time 18.0 hour |
in ASTM #2 Oil |
DuPont Elvax® 40L-08 Low Smoke Non-Halogen Jacket Formulation
(discontinued **) Elvax® 40L-08 low smoke non-halogen jackets.Information provided by DuPont. |