Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.99 MPa | 1594 psi | JIS-K-6723 |
Denka REOMER G G8053 Thermoplastic Elastomer, For Injection Molding Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |