Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 1040 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 7.20 MPa
1040 psi
ISO 37
PolyOne OnFlex™ S EF 60A-3S1967 Thermoplastic Elastomer (TPE)
OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell..
Tensile Strength at Break 7.20 MPa
1040 psi
ISO 37
PolyOne OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE)
OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p..
Tensile Strength at Break 7.20 MPa
1040 psi
ISO R 527
Stir SpA E 2092 65 (PVC)
Application: Extrusion for seals and profilesInformation provided by STIR SpA
Tensile Strength at Break 7.17 MPa
1040 psi
ASTM D412
Teknor Apex APEX® 1519-39 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMForms-PelletsFeatures- Good flexibility Information provided by Teknor Apex Company
Tensile Strength at Break 7.17 MPa
1040 psi
ASTM D638
Teknor Apex Telcar® 90-E607B-75NT Ethylene Vinyl Acetate Copolymer
Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several..
Tensile Strength at Break 7.17 MPa
1040 psi
ASTM D412
Teknor Apex Telcar® OBC 4876N Thermoplastic Elastomer
Uses: Flexible Grips; Overmolding; Soft Touch Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:..
Tensile Strength at Break 7.17 MPa
1040 psi
ASTM D412
Teknor Apex Uniprene® UN-7100-73 Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Tensile Strength at Break 7.20 MPa
1040 psi
ISO 37
ELASTO UK Dryflex® 5049-110 TPE, Modified Injection Molding Grade for Auto Mud Flaps
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5049-110 is specifically designe..
Tensile Strength at Break 7.20 MPa
1040 psi
ASTM D638
ELASTO UK Dryflex® 650450 TPE, Improved Compression Set and High Temperature Resistance, 45A Hardness
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi..
Tensile Strength at Break 7.17 MPa
1040 psi
ISO 37
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 7.17 MPa
1040 psi
ISO 37
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 7.18 MPa
1040 psi
Longitudinal; ASTM D3759
3M Scotch® 681 Transparent Film Tape
Scotch® Tape 681 is an excellent high tack, transparent film tape used for various packaging applications such as temporary holding, combining, light-duty carton sealing, bag sealing, and attaching..
Tensile Strength at Break 7.16 MPa
1040 psi
ASTM D412
3M Scotchcast™ 2131 Flame-Retardant Compound
3M Scotchcast Flame-Retardant Compound 2131 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. It formulation makes it particu..
Tensile Strength at Break 7.17 MPa
1040 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 181-64MED Thermoplastic Elastomer  (discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grades. ..
Tensile Strength at Break 7.17 MPa
1040 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 101-60W261 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Copyright © lookpolymers.com All Rights Reserved