Polymer Property : Tensile Strength at Break = 11.44 MPa
Polymer Property :
Tensile Strength at Break =
11.44 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
11.44
MPa
1659
psi
ISO R 527
Stir SpA A 58 AT (PVC)
Application: Foamed intersoleInformation provided by STIR SpA