Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 772 MPa | 112000 psi | Plate |
Special Metals INCONEL® alloy 22 Austenitic Alloy INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperat.. |