Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.839 MPa | 1137 psi | ASTM D 412 |
CPT C-Flex® R70-046 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |