Polymer Property : Tensile Strength at Break = 12.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.2 MPa

@Temperature 23.0 °C
1770 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 361-0190 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - UL 94 HB compliantPu..
Tensile Strength at Break 12.2 MPa
1770 psi
ASTM D638
ExxonMobil Escorene® LD 725.21 Molding, extrusion, compounding and adhesive resin  (discontinued **)
Escorene Ultra LD 722.21 is 18 wt% vinyl acetate copolymer suitable for molding, extrusion, compounding and hot melt adhesive applications.Information provided by ExxonMobil Chemical
Tensile Strength at Break 12.2 MPa
1770 psi
ASTM D638
LyondellBasell Purell® PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding
Purell PE 1840 H is a low density polyethylene with good flexibility and is delivered in pellet form. It is designed for small blow molding but can also be used in film applications and injection mo..