Polymer Property : Tensile Strength at Break = 120000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 655 - 827 MPa
95000 - 120000 psi
ThyssenKrupp X8Ni9 Structural Steel
Data applies to plate thicknesses from 13/64 to 1 15/64 in.9% nickel steel for low temperature service down to -320°FApplication for pressure vessels and tanks for the transportation and storage of..